{"id":280,"date":"2024-08-05T12:22:12","date_gmt":"2024-08-05T04:22:12","guid":{"rendered":"http:\/\/www.1.com\/?p=274"},"modified":"2024-10-10T13:16:29","modified_gmt":"2024-10-10T05:16:29","slug":"about-detail-67","status":"publish","type":"post","link":"https:\/\/www.hexinmusu.com\/de\/about-detail-67.html","title":{"rendered":"Niederdruckgussverfahren"},"content":{"rendered":"
<\/figure>\n\n\n\n

\u4f4e\u538b\u94f8\u9020\u662f\u5728\u538b\u529b\u4f5c\u7528\u4e0b\u586b\u5145\u6db2\u4f53\u91d1\u5c5e\u5f62\u6210\u94f8\u4ef6\u7684\u4e00\u79cd\u65b9\u6cd5\u3002\u5b83\u88ab\u79f0\u4e3a\u4f4e\u538b\u538b\u94f8\uff0c\u56e0\u4e3a\u5b83\u4f7f\u7528\u7684\u538b\u529b\u5f88\u4f4e\u3002\u5de5\u827a\u6d41\u7a0b\uff08\u89c1\u56fe1\uff09\u4e3a\uff1a\u5728\u5bc6\u5c01\u5769\u57da\uff08\u6216\u5bc6\u5c01\u94bb\uff09\u4e2d\uff0c\u8fdb\u5165\u5e72\u538b\u7f29\u7a7a\u6c14\uff0c\u91d1\u5c5e\u6db22\u5728\u6c14\u4f53\u538b\u529b\u4e0b\uff0c\u6cbf\u5347\u7ba14\u4e0a\u5347\uff0c\u901a\u8fc7\u6d47\u53e35\u5e73\u7a33\u8fdb\u5165\u81548\uff0c\u4fdd\u6301\u5769\u57da\u5a31\u4e50\u6db2\u538b\uff0c\u76f4\u81f3\u94f8\u4ef6\u5b8c\u5168\u51dd\u56fa\uff0c\u7136\u540e\u7f13\u89e3\u6db2\u538b\uff0c\u4f7f\u5f00\u53e3\u7ba1\u672a\u51dd\u56fa\u91d1\u5c5e\u6db2\u6d41\u5769\u57da\u574d\u584c\uff0c\u7136\u540e\u901a\u8fc7\u7f3812\u5f00\u542f\u94f8\u4ef6\u3002
Die Verfahrensspezifikationen f\u00fcr das Niederdruckgie\u00dfen umfassen die Beschickung, die Druckbeaufschlagung, die Vorw\u00e4rmtemperatur, die Einspritztemperatur, die Schlichte, usw.<\/p>\n\n\n\n

(1) Aufladung und Druckbeaufschlagung<\/h2>\n\n\n\n

Der Steigdruck ist der Druck, der erforderlich ist, wenn der Pegel der Metallfl\u00fcssigkeit bis zur Durchfluss\u00f6ffnung ansteigt. Die Steiggeschwindigkeit der Metallfl\u00fcssigkeit im Steigrohr sollte so langsam wie m\u00f6glich sein, damit das Gas im Hohlraum entweichen kann und das Metall beim Eintritt in die Durchfluss\u00f6ffnung nicht spritzt.<\/p>\n\n\n\n

(2) F\u00fclldruck und F\u00fcllgeschwindigkeit<\/h2>\n\n\n\n

Der F\u00fclldruck Pa ist der Druck, der erforderlich ist, um die fl\u00fcssige Metallcharge an die Oberseite des Gussteils zu heben. W\u00e4hrend der F\u00fcllphase ist die Geschwindigkeit des Druckanstiegs auf der vollen Fl\u00fcssigkeitsoberfl\u00e4che die F\u00fcllgeschwindigkeit<\/p>\n\n\n\n

(3) Druckbeaufschlagung und Geschwindigkeit der Druckbeaufschlagung<\/h2>\n\n\n\n

Nach dem fl\u00fcssigen Metall gef\u00fcllt Hohlraum, weiterhin den Druck zu erh\u00f6hen, so dass die Kristallisation des Gusses in einer bestimmten Gr\u00f6\u00dfe von Druck Erstarrung. An diesem Punkt wird der Druck als Kristallisationsdruck bezeichnet. Je h\u00f6her der Kristallisationsdruck ist, desto besser ist der Schrumpfungseffekt, und desto dichter ist das endg\u00fcltige Gussgewebe. In jedem Fall kann der Kristallisationsdruck nicht erh\u00f6ht werden, um die Qualit\u00e4t der Gussst\u00fccke zu verbessern.<\/p>\n\n\n\n

(4) Haltezeit<\/h2>\n\n\n\n

Der Werkzeuginnendruck wird auf den Produktdruck erh\u00f6ht und f\u00fcr eine bestimmte Zeit auf dem Kristallisationsdruck gehalten, bis das Gussteil vollst\u00e4ndig erstarrt ist. Die erforderliche Zeit wird als Nachdruckzeit bezeichnet. Wenn die Druckzeit nicht ausreicht, ist das Gussteil nicht vollst\u00e4ndig erstarrt, Hohlraum Metall fl\u00fcssig alle oder einen Teil der Str\u00f6mung zur\u00fcck in die Spende, was zu Gussteilen \"leer\" Bericht: wenn die Druckzeit zu lang ist, bleibt das Gussteil zu lange, nicht nur die Ausbeute des Prozesses zu reduzieren, sondern auch dazu f\u00fchren, dass der Mund der Str\u00f6mung \"Einfrieren\", so dass das Gussteil ist schwer zu bilden. Gussteile sind schwer zu formen, daher muss die Produktion die richtige Druckzeit w\u00e4hlen.<\/p>\n\n\n\n

(5) Gie\u00dftemperatur und Vorlauftemperatur<\/h2>\n\n\n\n

\u4f4e\u538b\u94f8\u9020\u53ef\u91c7\u7528\u5404\u79cd\u94f8\u9020\u7c7b\u578b\uff0c\u975e\u91d1\u5c5e\u5de5\u4f5c\u6e29\u5ea6\u4e00\u822c\u4e3a\u5ba4\u6e29\uff0c\u9996\u5148\u662f\u7279\u6b8a\u8981\u6c42\uff0c\u91d1\u5c5e\u5de5\u4f5c\u6e29\u5ea6\u6709\u4e00\u5b9a\u8981\u6c42\uff0c\u5982\u4f4e\u538b\u94f8\u9020\u94dd\u5408\u91d1\uff0c\u91d1\u5c5e\u5de5\u4f5c\u6e29\u5ea6\u4e00\u822c\u63a7\u5236\u5728200~2500C\uff0c\u6d41\u52a8\u8584\u58c1\u590d\u6742\u90e8\u4ef6\uff0c\u53ef\u8fbe300~3500C\u3002\u5173\u4e8e\u5408\u91d1\u7684\u6d47\u7b51\u6e29\u5ea6\uff0c\u5b9e\u8df5\u8bc1\u660e\uff0c\u5728\u786e\u4fdd\u94f8\u4ef6\u5f62\u6210\u7684\u524d\u63d0\u4e0b\uff0c\u5e94\u5c3d\u53ef\u80fd\u4f4e\u3002<\/p>\n\n\n\n

(6) Beschichtungen<\/h2>\n\n\n\n

Wenn Niederdruckguss aus Metall verwendet wird, muss er zur Verbesserung der Lebensdauer und der Gussqualit\u00e4t beschichtet werden; die Beschichtung sollte gleichm\u00e4\u00dfig sein, und die Dicke der Beschichtung sollte entsprechend der Oberfl\u00e4chenbeschaffenheit des Gussteils und der Gussstruktur festgelegt werden.<\/p>","protected":false},"excerpt":{"rendered":"

\u4f4e\u538b\u94f8\u9020\u662f\u5728\u538b\u529b\u4f5c\u7528\u4e0b\u586b\u5145\u6db2\u4f53\u91d1\u5c5e\u5f62\u6210\u94f8\u4ef6\u7684\u4e00\u79cd\u65b9\u6cd5\u3002\u5b83\u88ab\u79f0\u4e3a\u4f4e\u538b\u538b\u94f8\uff0c\u56e0\u4e3a\u5b83\u4f7f\u7528\u7684\u538b\u529b\u5f88\u4f4e\u3002\u5de5\u827a\u6d41\u7a0b\uff08\u89c1\u56fe1\uff09\u4e3a\uff1a\u5728\u5bc6\u5c01\u5769\u57da\uff08\u6216\u5bc6\u5c01\u94bb\uff09\u4e2d\uff0c\u8fdb\u5165\u5e72\u538b\u7f29\u7a7a\u6c14\uff0c\u91d1\u5c5e\u6db22\u5728\u6c14\u4f53\u538b\u529b\u4e0b\uff0c\u6cbf\u5347\u7ba14\u4e0a\u5347\uff0c\u901a\u8fc7\u6d47\u53e35\u5e73\u7a33\u8fdb\u5165\u81548\uff0c\u4fdd\u6301\u5769\u57da\u5a31\u4e50\u6db2\u538b\uff0c\u76f4\u81f3\u94f8\u4ef6\u5b8c\u5168\u51dd\u56fa\uff0c\u7136\u540e\u7f13\u89e3\u6db2\u538b\uff0c\u4f7f\u5f00\u53e3\u7ba1\u672a\u51dd\u56fa\u91d1\u5c5e\u6db2\u6d41\u5769\u57da\u574d\u584c\uff0c\u7136\u540e\u901a\u8fc7\u7f3812\u5f00\u542f\u94f8\u4ef6\u3002\u4f4e\u538b\u94f8\u9020\u7684\u5de5\u827a\u89c4\u8303\u5305\u62ec\u5145\u7535\u3001\u589e\u538b\u3001\u9884\u70ed\u6e29\u5ea6\u3001\u6ce8\u5c04\u6e29\u5ea6\u3001\u94f8\u9020\u6d82\u5c42\u7b49 (1)\u5145\u578b\u548c\u589e\u538b \u5347\u6db2\u538b\u529b\u662f\u6307\u5f53\u91d1\u5c5e\u6db2\u4f4d\u4e0a\u5347\u5230\u6d41\u53e3\u65f6\u6240\u9700\u7684\u538b\u529b\u3002\u91d1\u5c5e\u6db2\u4f53\u5728\u5347\u6db2\u7ba1\u4e2d\u7684\u4e0a\u5347\u901f\u5ea6\u5e94\u5c3d\u53ef\u80fd\u6162\uff0c\u6709\u5229\u4e8e\u578b …<\/p>","protected":false},"author":1,"featured_media":470,"comment_status":"open","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":[],"categories":[21],"tags":[47,49,89],"class_list":["post-280","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-about-news","tag-low-pressure-casting","tag-die-casting","tag-aluminium-alloy"],"_links":{"self":[{"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/posts\/280","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/comments?post=280"}],"version-history":[{"count":0,"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/posts\/280\/revisions"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/media\/470"}],"wp:attachment":[{"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/media?parent=280"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/categories?post=280"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.hexinmusu.com\/de\/wp-json\/wp\/v2\/tags?post=280"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}